    Hi Daniel, Do you know about using hydrogen peroxide added to
    sparex-type pickle for removing copper plating? Reactive Metals
    publishes a paper about it.  Here's the off-the-top-of-my-head
    too-lazy-to-go-find-the-paper summary: Take some hot pickle, put your
    work in.  Add hydrogen peroxide until you see some bubbling.
    (proportions vary according to the strength of the chemicals and
    temperature.)  Let sit for a minute or two.  Take out the work, scrub
    it off (toothbrush, brass brush, scotch brite pad, pumice, or
    whatever...).  Repeat as necessary.  This gets into the crevices
    better than simple abrasion.  Take care not to forget it in the
    solution, as it will etch the surface in that case.  As always, use
    good ventilation. (side note to the person who asked about
    ventilation: A fan blowing out the window is the cheapest option. 
    Make sure your soldering station or whatever you are ventilating is
    between you and the ventilation.  The next cheapest option is to buy
    a bathroom vent fan, and install in a a window or hole in the wall.) 

    I suppose you could experiment, and see if it works to add hydrogen
    peroxide to citric acid?  If you do, let us know the result! Cindy
    www.cynthiaeid.com  


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project