========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Cherie, You need to run your Stainless steel shot with Super Sheen burnishing compound or something similar. This combination should give you a nice burnished finish. To take it a few steps further, you can run silver items through a product called Shell shine green and finally an absorbent cob meal. The last two processes are run dry. The shell shine green is a fine Walnut shell which contains a chrome oxide polishing compound. This will give a fine/high polished finish. The cob meal is the last step which removes any residue left from the dry, chrome oxide media. You only need to run the last step for about 1-2 hours. If you need further information on these processes, Rio Grande has a technical support department to assist with questions like this. Phillip Scott G.G. Technical Support & Sales Rio Grande ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project