| Re: [Orchid] Frustrated reticulation & fusing | ||
|
[Thread Prev]
[Message Prev]
[Date Index]
[Thread Index]
[Message Next]
[Thread Next]
From: William Denayer Date: Sun Mar 09 22:18:59 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Sue, I had the same problem (with 22 ga and the little torch). I found excellent information about reticulation at the website of Hoover and Strong (see 'articles' or do a search). There is also an article on reticulation in their catalog, but the article on the net is better and more into detail. It worked for me. Regards, Will ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project