    I am a self-taught silver/goldsmith. I decided to experiment with
    trying to reticulate the face of a piece of 16 gauge silver. I have
    a Little Torch. I used Tip #6 and a large, bushy flame. I believe I
    heated the piece for at least 30 minutes and could never get the
    surface melted. 

    Also, this weekend I decided to try fusing some pieces to a sheet to
    make a bracelet. The first attempt was 22ga backing with 22ga pieces
    to be fused on the surface. I could melt the pieces and make the
    curl up, but I could never get the pieces to fuse to the backing. I
    used #6 tip and heated evenly both front and back--moving the torch
    pretty constantly. I then tried to fuse the same 22ga pieces to a
    backing of 32 gauge silver. Never made it! 

    Do I have the wrong torch for reticulation and large-scale fusing?
    What else could be wrong? 

J. S. (Sue) Ellington


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project