Hi Dayananda,

    What temperature are you wanting to reach? If you just want to get to
    about 2100 deg F a NeyTech furnace will work. Otherwise you will be
    spending over $3000 to get to any temperature between 2100 and 3000
    deg F. This element will not last more than a year running at this
    temperature. So if you go with this oven you will have to accept this
    additional cost and work it into your pricing. 

    I have a customer in Helena, MT that is doing this and he is using a
    NeyTech furnace with a digital controller that I installed. It is
    working but the limitation is the heating element. In order to get a
    higher temperature an exotic heating element needs to be used and
    they are much more expensive and fragile. 

    I can give you more info as far as ovens that reach the higher
    temperatures if you are interested. Contact me off the list either by
    email or toll free at 1-877-262-2185. 

Thanks,
Ken Kotoski
MPG Repair
www.mpgrepair.com
1-877-262-2185


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project