    It will depend on how the platinum ring was made and what alloy of
    platinum it is made from ( there are at least half a dozen in common
    use in the US). Some platinum alloys approach medium carbon steel
    for hardness and are harder than any other common jewelry metal  but
    the majority of cast platinum rings are very soft and scratch. bend
    and dent easily. On the white gold side it also depends on the
    alloy. Nickel white golds are quite hard and will not easily dent or
    bend. The down side is that they are not very white and are in need
    of Rhodium plating to look "white" so the plating wears off fairly
    fast and the ring ceases to look very good where it is worn. Also a
    significant portion of the population has a severe skin reaction
    with nickel and will not be able to wear it.  Most palladium white
    golds are grey (just a little bit darker than platinum) not white
    but they are much softer than nickel white. So It all depends on
    what alloys you are referring to. 

Jim

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project