From: Jack
Date: Thu Mar 06 22:22:43 2003
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


    Allan, sorry to differ (unless Australian legislation is different)
    but the 7.5% in sterling can be anything - copper is most
    traditional, but not stipulated. So as long as 92.5% of the contents
    of an alloy by weight are silver then it is sterling. 

    Don't quite follow your logic re 24 K gold, but in all these things
    (silver qualities, Karat gold etc) the proportions are by weight not
    volume so yes, in theory, you could mix about 11 buckets of tin
    (light metal - haven't checked the maths, but I'm talking
    theoretically:)) to 1 bucket of 24 K gold and still have an alloy
    that could legally bear a UK 9 K hallmark. 

Jack Ogden


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project