| Re: [Orchid] About ".835" | ||
|
[Thread Prev]
[Message Prev]
[Date Index]
[Thread Index]
[Message Next]
[Thread Next]
From: Martin Niemeijer Date: Wed Mar 05 22:10:04 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hello mark 835 is what we mark as second grade silver 835/1000 when we do not want hallmark jewelry Hallmarking is bringing extra costs and a lot of customers do feel the need for it. So it was probably silver with a thick gold plating greetings Martin Niemeijer N design Molenkreek 23 8032 JK Zwolle Netherlands ndesign AT wishmail.nl +31 (0)38 4539203 +31 (0)6 51831576 ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project