    Hi Cherie...Grisaille loosely translated is "variations of gray" In
    Europe during the middle ages to renaissance a  style of painting
    thin layers of white enamel over a black background was developed .
    The thinner and fewer the layers in one area the darkest the
    grey...more layers whiter.  Some areas were scraped back into the
    unfired white layers to reveal  the previous layers. there was also
    some embellishment with gold and/or transparent color.  Oppi
    Untracht's book was the first source of info for me.  In my ignorance
    I developed my own technique, which uses dry rather than painted
    enamels.  I worked in just this grisaille technique for 12-13 years
    but since then have incorporated a lot of foils and transparent color
    in my work  in conjunction with grisaille sometimes, sometimes by
    itself.  DX Ross is another Grisaille artist...she works in the
    painted technique.  have fun and don't worry over much about rules! 
    Marianne hunter

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2007, The Ganoksin Project