    Regarding asbestos sheets. Are you lining your crucible or your
    flask? I am a lurking dentist. In dentistry we line our flasks prior
    to investing with strips of thickish asbestos prior to investing. As
    memory serves this is to lessen the shrinkage in the cast crown or
    bridge. I have never used this in casting any jewelry. It was a must
    in dental school. I am sure that dental lab supply houses such as
    Kerr have this or a non asbestos substitute. I believe anyone with a
    wholesale number will be able to purchase from them. In lieu of that
    you may find a friendly dental lab that can help. Also try the
    dental supply houses in the phone book. In regards to burnishers. We
    dentists use these in all shapes and sizes. If you can access a
    dental catalog they will be listed under "operative dental 
instruments" 
    Hope this helps, Mary.

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2007, The Ganoksin Project