From: Renate Sommer Date: Mon Mar 03 00:56:40 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I feel I really should chip in here. I am surprised that no-one has mentioned the possible dangers associated with asbestos. Is this not an issue in America? Have the Australians possibly gone too far in their fear of the dangers of breathing in asbestos fibres? Has there been a climate of fear built around asbestos here and the dangers of contracting mesothelioma? Don't want to scare anyone, but if you say "asbestos" in Australia, someone else says Aaaaarrgghh! I'm very fond of you clever Orchideans (and those just learning) and would hate you to subject yourselves to danger. On the other hand I am aware of the possibility of being manipulated by the result of a one or two emotive stories in the media and the rest of the population becoming paranoid. I would be interested in your opinions on this subject, as I have put sheet asbestos to good use in the past and sometimes wish I could find something to do the same job that is not so dangerous. Cheers for now, Renate, Adelaide, Australia ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2007, The Ganoksin
Project