From: Gerald Alexander Livings Date: Mon Mar 03 00:29:58 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > My father has recently made up a press to press out > mower blades. I was just wanting to know if you had any information > on how we would go about hardening them Any information that you > could send would be most helpful. Darren McGinty Darren, first, what your asking about is more in the realm of industrial fabrication and manufacturing. I would suggest that you go to the library and ask at the reference desk about a set of 20 or so books called the Th omas register. If you can think of something, this book will have a listing of companies that make or sell it, even jewelry. You will find companies that specialize in hardening and tempering so tha t the blades that your dad makes will be uniformly hardened. Have you thoug ht about what will happen if an improperly tempered blade hits a rock at hig h speed? In this day and age of lawsuits you will want very good liability insurance. there will also be listings of companies that sell this type of coverage. I use this register sometimes when I am brainstorming about a project. I hope I gave you some good advice and directions to go. good luck! Honorably, Gerald A. Livings ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2007, The Ganoksin
Project