========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > A simple fundamental mistake many self taught jewelers make is > to use easy solders were you should be using a hard solder. Easy > solder is not easier to use. Hard solder is not hard to use. It > often makes a job more difficult as you have found out. Keep you > seam really tight and use the highest flow temperature solder > possible. For 14kyg sizing I recommend 14ky hard or 14ky weld. For > 14kwg rings use 19kw weld or 20kw weld. This will help > dramatically. Other things to look for. Again, keep you seam really > tight. Keep your flux and flux brush clean. Be sure to use a boric > acid and alcohol dip and a secondary flux such as batterns directly > on the solder joint. Good luck John Sholl Littleton, Colorado This is highly confusing to me. Firstly, what is "19 or 20k weld"? I have never heard of this grade of solder. Also, I thought that only lower karat golds could be used as solders on a given object. Please help me to clarify this for myself. I don't want to perpetuate any misinformation, if my previous understanding is erroneous. Thanks. Danny Rondeau ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project