Date: Tue Feb 25 23:28:22 2003
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


    As a rule of thumb, I'd stay away from most soluble metals in a
    fresh or salt water aquarium, especially iron (steel), copper, etc. 

    That being said,  copper sulphate solution was (maybe still is) one
    of the old standby treatments for fish disease in salt water
    aquaria. It was used to treat parasites such as saltwater "ich" and
    "velvet" (oodinium), without harming the fish.  It worked wonderfully
    w/ one major caveat: it was deadly to invertabrates, such as those
    found in reef tanks, including crabs, clams, shrimp, sea anemones and
    urchins, corals, etc.  (This is why sea going ship and boat hulls
    were painted w/ a copper based coating: deadly to barnacles, sea
    worms, etc.) 

    If a fresh water aquarium contains freshwater inverts such as
    crayfish, red fiddler crabs, etc., and there is significant soluble
    copper present, they will die. 

    Also:  if a piece is hollow, make sure that is pickle free.  Sparex,
    etc. might readjust the ph down and out of the comfort range of
    certain fish. Old pickle also contains copper. 

    Good luck, sounds like an interesting project. 

Andy

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project