    Kitty  - There are several things to consider in tumble finishing 
    your dichroic glass jewelry. 

    First - the tumble vibe 5 is not robust enough to "turn" steel shot,
    you need to use a rotary tumbler for that.  A small rotary rock
    tumbler with flat internal sides should cost under $100. 

    Second - I'd strongly advise you to use the stainless steel shot. 
    You will buy it eventually, after the carbon steel shot gets a bit
    of rust and ruins a batch of your jewelry. 

    Third - I just talked to Gene Lacey, a dichroic glass jeweler here
    in the Denver area, and she sets her glass in sterling, then runs it
    in an abrasive media in a small vibratory tumbler, similar to the
    Tumble Vibe 5.  She finishes the jewelry with stainless steel shot
    in a small rotary tumbler.  The glass after firing will withstand
    those processes with no problem. 

    I'd make the loop prior to tumbling. 

    Self serving blurb - my fourth edition of Tumble Finishing for
    Handmade Jewelry is now available.  Rio Grande has a supply and
    several other dealers will also be carrying it.  I think Hannuman is
    going to provide some excerpts for the list. 

Judy  Hoch, G.G.
judy AT marstal.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project