From: daniel rondeau Date: Fri Feb 21 20:18:35 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== In a previous post (old news by now) the author notes; "photopolymer systems (eg Colorit,UltraUV)...cure at roughly room temperature using actinic light." My question is three-fold. What is "UltraUV" compared to Colorit? I have been unable to find this product in a net search. Is it only available in the US? If these photo-activated ceramic polymers are cured with actinic light, can an enterprising jeweller substitute an aquarium actinide lamp for the expensive Colorit setup? And finally, can the same enterprising and thrifty person buy a sheet of red-tinted acrylic plastic and form it into the also expensive light shield supplied with the Colorit system? (Presumably, this is to keep the blue end of the spectrum of natural or incandescent light from begining to cure the polymer while the jeweller is still applying it to the piece.) Thanks for any thoughts or encouragement- should I happen to be the first to have thought these crazy cheap-outs would work. Danny Rondeau ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project