    Hi Peter I've always been aware of scale and stain, having been in
    this business for over 25 years.  I've long known how to deal with
    it, both preventing and removing, when I am soldering.  Until
    recently, my silver production was small and mostly limited to
    fabricated pieces.  Now I am producing a small line of charms and
    other pieces that are cast in silver.  I don't do my own casting for
    a lot of reasons, so I am sending the work out to a contractor. On
    the smaller pieces, the stain is so deep that I can't remove it
    without destroying the detail, or wearing through thinner areas.  I
    have no control over their casting process, so it remains for me to
    remove the stain afterwards.  Any suggestions?  I have used their
    'low-oxidizing' silver, which gives much better results, but it is
    much softer.  This is acceptable on some pieces, not on others. It is
    also harder to intentionally oxidize on those pieces that need it.
    Thanks, Jim


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project