    Hi Karen, I make a version of the spinner ring.  So it's best to The
    bottom band is flared slightly on the edges to hold the spinning
    band like this: I make the base band -solder it sized slightly
    smaller than the finished size I want. Then I make a narrower,
    spinning band that is just barely larger than the outside diameter
    of the base band so that when it is soldered closed it will just slip
    over the base. With the spinner band in place  on the base ring( you
    might want to tape it or something) I lay the ring on its side on a
    smooth steel plate, set the ball of a ball pein hammer on the side
    facing up - and then strike the flat of the hammer with a mallet
    basically - I don't have a hydraulic press or other means to flare
    the band - so I am using a ball pein that is sufficiently large that
    it doesn't protrude from one side of the ring to the other - and yet
    small enough that it can fit into the ring a bit and flare the
    edges. I flip the ring from one side to the other, flaring a bit at a
    time on both sides and testing that the spinning ring will still
    spin. The flaring process usually stretches the ring about a 1/4 of a
    size. There's a picture of the ring on my site
    www.sumiche.com/platinum.html that might make the procedure seem
    clearer. best, Michelle 


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project