    My welding supply store warns AGAINST using a soapy water solution
    to check for leaks on bottled gases, especially oxygen...UNLESS one
    is absolutely certain that it is a NON PETROLEUM based soap being
    used such as liquid Ivory. 

    I can't relay their explanation in detail but the jist of it has to
    do with the gases moving into the regulators with such
    speed/pressure (especially the oxygen.) that the "friction"
    generates enough heat to ignite petroleum residue. They note of
    course that this is undesirable since open flame and bottled gases
    don't mix well. 

    This said I will be the first to admit that I have for years used
    "any old liquid soap" and water mixture to test propane connections
    and have had no problems. But believing that old dogs can learn new
    tricks...sometimes, I have heeded the warning and now use only
    non-petroleum based liquid soap. Can't be too safe with these gas
    setups! 

    (The welding shops also sell bottles of safe solutions for leak
    testing .) 

    Usual disclaimers... 

    Joe Battle Ground, WA where it's unseasonably sunny and warm.

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project