    Ginger, The elks teeth you are referring to are generally called
    "whistlers" . At least that's what they are called here in Kodiak
    Al;aska. To prepare them for mounting simply cut the lower part off
    across the long axis of the tooth  with a jeweler's saw making a
    sort of cabochon and set as you would a stone. Polishing is not
    really necessary as the elk has done it for you, although it
    wouldn't hurt to give it a final buffing after setting.  I'm sure
    someone has done it at one time or another, but I have never seen 
    the tooth used whole.  The root is not particularly attractive and
    if it were to be set as a pendant, root and all,  the patterned end
    would be on the bottom and not really visible. Having said that,  I
    have seen them used  as  watch chain ornaments bearing the insignia
    of the Benevolent and Protective Order of Elks. These  have had most
    of the root cut off and then been capped with a  fairly wide gold 
    cap  which was probably cast from a wax individually made for the
    tooth. Jerry in Kodiak

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project