    Hello Ian, Titanium is really not dangerous. It is even used as body
    implants, such as repairing broken bones with plates and screws. So
    the arthritis story is what we in the Netherlands call (translated) a
    slice of bread with ape meat. So complete bullshit. 

    Titanium is only a little dangerous if you are grinding it. But
    every grinding dust and metal dust should not be unhealed. This
    counts also for gold dust. 

    An other thing, titanium is a reactive metal.  Reactive means that
    the metal easy reacts with oxygen. The effect is that small titanium
    parts will burn. Like iron filings in a flame. and the magnesium
    strips in the Physics lesson at school. So if you are milling it or
    grinding this metal be aware of that small parts are inflammable. 

    The reactive effect of this metal is the reason that this metal is
    hypoallergenic. The oxide layer occurs extreme rapid on the surface.
    If you are sanding titanium the oxide is instant occurring direct the
    sanding cloth on the open metal surface. Also the oxide layer is so
    close that no metal ions will fade out the surface. And this makes it
    very suitable for body implants. 

    Just use your titanium and make nice thins of it. 

greetings
Martin Niemeijer
N design
Molenkreek 23
8032 JK Zwolle
ndesign AT wishmail.nl
www.ndesign.nl
+31 (0)38 4539203
+31 (0)6 51831576

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project