From: wemery Date: Thu Dec 05 22:20:14 2002 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== You can make a VERY close estimate of the amount of gold in a quartz specimen quite easily If you have a long narrow graduated lab flask (graduated in cm), fill it half full with water Drop in the specimen to learn the volume in cubic centimeters Weigh the piece in grams The specific gravity of quart z is 277 That is, the specific gravity of quartz is 277 grams per cc Multiply the volume of the specimen x 277 and record this figure Le t's say the volume of the specimen is 84 cc's 84 x 277 233 (grams) But when you weighed it, the piece weighed 37 grams The extra weight is attributable to the gold 37 grams - 233 grams 137 grams I f the specific gravity of pure gold is 193, then 137 grams / 193 grams 0,71 grams of gold in the specimen Now, if you DON'T have a graduated flask in which to the measure the volum e of the specimen, you need to calculate the volume using some solid geometr y methods If you have a CAD program like Matrix (wwwgemvisioncom), and the piece is of a shape that you can fairly closely reproduce, Matrix will calculate the volume of the solid object for you and will calculate the weight as well, so you don't even need a scale! Matrix rules Wayne Emery ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project