    Peter, To get an approximate calculation of the gold content in
    quartz this is what you would do: 

    A) Figure out the volume of the quartz/gold specimen. This is
    easiest done using water displacement. Or by weighing in air and
    then in distilled water. (There are special scales that do this.)
    Subtract one weight from the other to give you the weight of the
    displaced water. Then you can find the volume of the specimen since
    we all know that one gram of distilled HOH is equal to a cubic
    centimeter. With this you can find the volume of the quartz/gold
    specimen. 

    B) Obtain the actual weight of the quartz/gold specimen. A triple
    beam will do. 

    C) Figure out what the specimen should weigh if it were pure quartz.
    This is done by using the known volume of the specimen and the know
    specific gravity of quartz. 

    D) To get the approximate weight of gold in the quartz/gold specimen
    you would then subtract the above C from the above B . The difference
    will give you an approximate weight of gold in the specimen. 

    This is only approximate since it cannot take into account any voids
    (hollow areas) in the specimen, other minerals present with
    different SGs, any metals alloyed with the gold, etc. 

    Hope that helps  : )  Steve Green / Rough and Ready Gems For all
    your colored gemstone BRIOLETTE needs and precision ultrasonic
    drilling. See us in Tucson at the GJX Show booth # 700, Feb 6th-11th
    2003 (across from the AGTA)

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project