    Dear Ed, I am particularly fortunate to own two books by E. Gubelin,
    the Swiss authority on gemstone inclusions. In his "Inclusions as a
    means of Gemstone Identification", GIA 1953, he devotes a long
    paragraph to Kashmir Sapphires. In his 

    "Internal World of Gemstones" ABC Zurich, 1983 he also devotes a
    paragraph to same. The most telling statement in the latter is
    "Kashmir sapphires are extraordinarily deficient in characteristic
    inclusions" He also stated that no single inclusion should ever be
    considered to be diagnostic as to origin in corundum varieties. He
    does, however, mention the fact that Kashmir sapphires are usually
    quite hazy, but the suggestion is that many localities have produced
    similar phenomena. He also states that the haziness may be due to
    liquid inclusions wihin microscopic fissures. 

    Of all the books that I treasure, Gubelins' works are the most
    fascinating.The more recent work is filled with perhaps the most
    spectacular micro photographs ever published. I noted that the price
    tag was still on the dust cover....it is the most I ever paid for a
    book.....$125.00 ! In todays dollars that would make it near $300.00
    !  ( It must have been a good poker day ! )  Ron at Mills Gem, Los 
Osos, CA. 

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project