========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hello Jean, Re your question: > i have just sprayed some 1 1/2 inch pierced copper disks with > plasti-kote hi-performance classic fast dry lacquer (no. 349) with > less than perfect results. ... some of the disks have an orange > peel texture, especially at the bottom half of the disk. There should be a phone number on the label for the company producing the lacquer. Give them a call and ask for the tech people or customer assistance. Those folks should understand the best techniques and parameters for your project. > what do you think caused the orange peel lacquer? i'm leaning > toward temperature, thinking that a higher temperature would allow > the lacquer to spread out a little more before it drys. I would think a higher ambient air temperature would make the finish dry more quickly. I've tried several spray lacquers, and have only found one that I'd recommend: G.J. Nikolas and Co. #2105 Clear Lacquer. It's made for polished silver, so might not be suitable for copper. You might try their company website for technical help. Hope this helps, Judy in Kansas Judy M. Willingham, R.S. Biological and Agricultural Engineering 237 Seaton Hall Kansas State University Manhattan KS 66506 (785) 532-2936 ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project