    Daniel Grandi: Thanks for your discertation as to the advantages of
    the Tivac inserts. I am planning on giving them a try. Currently I am
    using perforated flasks and can only fit four 4X6 flasks in my oven
    at one time. I figured that by using standard flasks with the Tivac
    inserts, I can fit nine 4X6 flasks at one time in my kiln. That alone
    will make the changeover worthwhile. 

    I also knock my castings out of the investment when cold to prevent
    cracking and also eleminates the need to dry the investment for
    disposal. I can imagine that the solid flasks with Tivac inserts will
    make knocking out the investment easier. 

    Thanks again for sharing your knowledge with us. As someone that has
    had to learn most of what I know the hard way, I appreciate the
    pearls of wisdom that you and others on this list share. Also special
    thanks to Hanuman for hosting this website. 

Ken Gastineau
Berea, Kentucky


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project