    Hey Brenda what H & S said sounds right, The first thing to look at
    is your thermocouples (pyrometer probe) they can go bad and or fail
    right out of the box, my experience is that as they age they read
    right at low temp but are off 100 or 200 =BA F above 1000 =BA F. I kee=
p a
    control or unused pyrometer just to test temperatures. I would need
    to see the orange peel surface, but it might be that your oven isn't
    reaching the peak temperature. (improper burnout due to worn
    thermocouple) 

    About the investment check with Kerr about its "Breakdown or Melting
    temperature" You might find its close to the casting temp. of the
    alloy. If that is the case you will have problems with the investment
    forming a hard layer on the cast part. 

    Also Hoover and Strong just hired a new metallurgist and
    Reformulated a lot of their alloys, the ones I use got better. 

Hope I helped some...
James M...
Outcast & Company
Seattle

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project