========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hey Guys: I just finished making waxes for wedding bands- my client wants to cast them in platinum. Here is my question- I have been told I should not make a mold by some friends saying it will seriously downgrade the design (my entire jewelry collection is casted from molds so I do not understand that logic) My other option I think is to make mulitple waxes of each ring and then cast because platinum is really tricky to cast and the castor may need several models to get it right (am I right on this one?) The rings that the client approved are a tiny bit big because I was going to make a mold but now since the seed has been planted in my brain that I should make multiple waxes now I am torn. Any suggestions and feedback from the orchid group would be great! dd ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project