>       I'm having difficulty maintaining a solidly resistant mask when
>     I etch copper and brass in ferric chloride using Press-n-Peel. Even
>     with a slow solution, the ferric chloride eats through the resist,
>     so that the area that is protected has pitting, similar to an
>     aquatint. 

    Joan, it's not anything you're doing wrongly. I was never able to
    make that stuff  work to produce anything other than a very poor
    "hobby-level' etch - and I've never seen anything that looked even
    halfway decent produced using it.  I would be delighted to be proved
    wrong however because that would mean I could then learn how to
    achieve satisfactory (to me) results, in the process saving
    considerable time and money. 

    Any outraged proponent of the stuff should feel free to email a 300
    dpi jpg to pictures AT netconnect.com.au of something with delicacy and
    depth that they've produced in this fashion. I don't expect to be
    inundated with pictures. <g> 

    Al Heywood  

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project