    From Alan Revere's book, Professional Goldsmithing: 

    Disk diameter for a hemisphere = (outside diameter - wall thickness)
    x 3.1415 x .92 

    so, if you want to make a 12 mm hemisphere from .7 mm sheet then
    subtract .7 from 12 and multiply this by 3.1415 (pi) and then by .9,
    divide by 2. This equals 16mm. 

    As Alan states in the book "the accuracy of this formula varies
    according to the technique of the goldsmith applying it."  This is
    because as you dap the shape it is possible to stretch the metal as
    you hammer, altering the metal.  Still it is as good a starting
    place as you will find. 

    I must seriously recommend that anyone interested in goldsmithing
    get Alan's book.  There is a lot of information here that is both
    inspiring and very handy.  

Larry

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project