From: ARands Date: Mon Jul 29 22:33:29 2002 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I'd be careful before using metal tea strainers in pickle. You might want to test it first by putting it in some pickle with a bit of scrap silver. If the strainer is not entirely stainless, you will get a copper coating on your silver. i have several strainers which are supposed to be stainless, but notice that there is some rust around the hinge areas. Mine are the kind that form a ball into which one puts the tea. . This is not a stain caused by the tea, but actual rust probably coming from the hinge pin. So do test yours to be sure that there is no possibility of contamination. Alma ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project