========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi All, I have some of the thermoplastic pellets which I have tried to use to hold my pieces while I set some stones in tube settings. It works well to hold the piece, but getting them out is a problem. If I reheat the whole thing, the plastic gets sticky and adheres to my piece and is the devil to remove. Will someone give me the correct way to use this wonderful stuff? And a warning to anyone who hasn't used it yet. Never use it with nail polish on, I found out that it creates a very strong bond and then you have three-D abstract art on your fingernails. Betty, In eastern pennsylvania where the heat just goes on and on. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project