    I am very keen to find a good alloy for 18crt white gold. My name is
    Alan Goldberg, and I am based in Melbourne, Australia. I have a
    casting problem with which I am desperately seeking some help. We are
    currently casting using a Mario Di Maio alloy that is nickle based (
    but meets the Euro regulations Re: nickle). We are having moderate
    success and would like to improve the quality. we use the alloy for
    all objects, But mainly rings and settings. Rings can range from 2
    to 12 gr ams. The main objective is to have an alloy that is cost
    friendly, soft enough for stone setting and ring sizing and also is
    as white as possible. ( Palladium based alloys are too expensive in
    this case.) The problem so far is that at times it casts absolutely
    porous-free and at other times (without changing anything), it looks
    like craters on the moon!! Even when it is absolutely blemish free,
    it is as hard as rock and very very very brittle. One wack with a
    mallet and it can crack into 2, and all this using a Nuetec Jzp???
    And also with a normal vaccuum assist, torch melted system,
    performing fantastically with all other metals. We have also tried
    using the manganese alloy from Precious Metal West, But this does
    not perform well with the Nuetec Machine. HELP. If anybody out there
    has anything they think could be a possible alternative for me,
    please let me thank you all in advance 

Alan Goldberg 

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project