========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== The dental industry has been casting nickel/cobalt and or chrome/cobalt aloys for years. the alloy had cost (10-12 years ago) about $9-15 per 16oz pound. Find a framework lab and you could probably get the "once cast" mistakes for the taking or a very low price. mix this metal with "virgin" metal to insure proper trace metal content. These alloys can be torch cast or induction cast. check with the lab tech as to technique for the alloys you get. Talladium, Ticonium, Vitalium and a host of lesser names are available. Hope this helps Mike & Dale, ultrasonicrepair.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project