From: Clinton Driggars Date: Thu Jun 06 00:44:13 2002 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > Hi, everybody, I need your help, I want to electroplate a > cooper jewelry piece with silver, but I don't know the procedure > for that. Does any body know something abut. I need to know if the > electrolitical solution can be made at home. Please excuse my > english. Sincerely yours: DENIS. Sure can, that is kind of a normal process. You can use a little nickel underneath or you can just use the silver over the copper. If you are just planning to do a small piece or just a few pieces then get a solution already made up, if you have an enormous amount to do then you could consider mixing your own. Let me know if you would like to join an electroplating group, or need info on a couple of suppliers for made up solutions at a reasonable price Clint D ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project