========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Donna, the yellow color you see in diamonds is caused by Nitrogen atoms replacing carbon atoms within the crystal lattice or crystal structure of the diamond. Nitrogen is the impurity, and the more Nitrogen atoms present, the more intense is the yellow. If I understand your question correctly, you believe that the yellow color in your diamond has become more intense over time. I have never heard of this happening, nor do I believe this is possible without special treatment. Maybe you are looking at your diamond under different lighting conditions, such as incandescent lighting instead of natural. Charles Heick Cincinnati, Ohio ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project