>      One very important thing the original poster needs to know is that
>     only diamond and ruby and sapphire can be retipped with the stone
>     in. 

    I know I have brought this up before but it obviously needs to be
    said again.  In today's treated gemstone market it is no longer safe
    to assume that you can heat ruby and sapphire.  So many treatments
    are being used that it is impossible to know what reaction might
    occur when heating these stones. I have had dyed rubies turn black,
    ruby doublets (from a very high end New York jewelry store who had
    apparently been fooled themselves as only some of the stones were
    doublets) split in two and fancy colored sapphires change color. You
    also need to thoroughly check diamonds for indications of fracture
    fillings before you go ahead and heat those stones as heating will
    most assuredly affect the treatment.  If it is at all possible we
    will always remove stones from their settings before retipping. 

Daniel R. Spirer, GG
Spirer Somes Jewelers
1794 Massachusetts Ave
Cambridge, MA 02140
617-491-6000
spirersomes AT earthlink.net
www.spirersomes.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project