    Hi, Tamara- You may need some trial and error on this, but if I were
    trying to polish a crystal with a dremel or other flexshaft without
    changing the shape, I would use diamond paste on soft cotton buffs.
    start with 600 grit diamond paste, follow with 1200, and then finish
    with the 14,000 grit diamond polish. Use a separate buff for each
    grit.  The best diamond polish I have found is called "super polish"
    and is available from a company called "Mountain Mist." 

    http://www.mtmist.org/ 

    The usual disclaimers follow, I am not affiliated with Mountain Mist
    and do not profit in any way from this recommendation, I am just a
    satisfied customer. 

    If you can't get a polish using this procedure, you may need to
    begin again starting with a 325 grit diamond paste, but you will want
    to proceed with caution if you do, because 325 grit is coarse enough
    to agressively carve into the crystal, and it sounds like you want to
    preserve the original shape. 

Lee Einer
http://members.cox.net/appealsman/

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project