| [Orchid] Quenching oil for steel | ||
|
[Thread Prev]
[Message Prev]
[Date Index]
[Thread Index]
[Message Next]
[Thread Next]
From: Kate Wolf Date: Sun May 12 23:00:07 2002 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi gang, We just wrapped up a delightful week of Knifemaking with Tim McCreight here. He's an inspiring teacher! We used O1 tool steel and hardened it in motor oil. What kind of oil do you all use to harden steel? (I am looking for something that won't go rancid and smells better than motor oil). Thank you! Kate Wolf in drizzly Portland, Maine http://www.katewolfdesigns.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project