    Regarding the proper ventilation for making glass beads, the
    question was "What do the experts think???   Which is the better way
    to go, respirators, and air cleaners, or a real and good exhaust
    system over or next to the are in which the beads are being made???" 

    Going on 15 years making glass beads here, and I will state
    unequivocally that for any kind of glass flamework, a positive
    exhaust system is absolutely essential. The amount of propane
    consumed is far higher than jewelers use, and there is a real serious
    risk of CO poisoning without adequate POSITIVE ventilation. The
    gasses from the fuel combusion must not only be exhausted, but there
    must be a positive intake of fresh air as well., as the glass working
    burners also deplete atmospheric oxygen. ("Positive" means by
    mechanical means, not just an open window.) If your friend is just
    wearing a respirator, she is courting disaster. 

    If you want to research the matter further, try visiting  
    http://www.isgb.org/cgi-bin/forum  and do a search in the archives
    using the key word "ventilation". There is no topic which has been
    discussed more thoroughly than this one, and all the "experts" agree.
    You need it. 

Rene Roberts

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project