    Greetings All, I haven't caught all the threads for this subject but
    what I have read seems very informative. It's pretty ironic that I
    was reading this months issue of Lapidary Journal and came across an
    article that covers this subject as well. The name of the article is
    'The Metallurgical Balancing Act' by Sharon Elaine Thompson. The
    article is quite enlightening probably because I am still learning.
    The article covers information about the alloys and some of the
    reasons certain ingredients are used and why the ratios are important.
    The dangers of recasting/re melting used gold or silver is also
    covered, but with a twist that I didn't know. Not only do you have
    problems due to depleted zinc and possible solder contamination but
    it seems that metals alloyed from different vendors can also give way
    to problems. If you get a chance read the article, it is very
    interesting, at least for me it was. By the way I do not work for
    Lapidary Journal nor do I have the pleasure of knowing Sharon Elaine
    Thompson. 

I'll be listening
Tom Timms
ttimms51 AT yahoo.com
USA Arizona

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project