From: Tony Date: Mon Apr 22 00:28:03 2002 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Sodium bisulphate (NaHSO3)is used for all sorts of processes including ceasing fermentation in cheap wine, but I've never heard of it for use in metalsmithing. I'd urge care. It decomposes very rapidly into sulfur dioxide gas (SO2) and sodium hydroxide (NaOH.) Most people are highly affected (this is NOT an allergy) by the gas which dissolves in the mucus of the lungs to form Sulphurous acid(H2SO3.) Result? Wheezing, tissue burn etc! Tony Konrath ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project