Hi Richard:

    Here's how I use my little double sided (round wire or flat sheet)
    ingot mold. 

    1. Warm the mold with the torch untill it's too warm to comfortably
    hold on to. 

    2. Lightly oil the inside of the mold using a cotton swab and
    machine oil or spray it lightly with "Pam" or another cooking oil
    spray.  Just the lightest coat possible, no dripping oil. 

    3  I light my torch without turning on the oxygen.  Just a big,
    bushy orange gas flame.  A candle will work too. 

    4. Holding the mold in the flame (with pliers if it's too hot), I
    cover all surfaces with soot from the flame. 

    5. Assemble the mold and heat it up again till once again it's too
    hot to touch.  You can test it with a wet bit of cloth.  If the water
    hisses a bit, you're at about the right temperature. 

    6. Melt, flux, and pour your metal into the mold.  Let it cool
    enough to handle it, and you're done. 

    I'll let someone else explain why it's done that way.  I just know
    it works for me, and I've tried it skipping some steps and didn't get
    as good results. 


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project