    I recently used a tig torch to weld copper, with both sil-phos
    brazing rod, and with ordinary copper wire. Now there's a colour
    match.  A tig torch is also called Heli-Arc by some, it's an electric
    arc process where the arc is surrounded by inert argon gas.  

    About the relationship of soldering, brazing, and welding: Soldering
    can be considered like glueing, but at low heat like 400-600.  
    Brazing is like the same, but high enough heat to get the material
    red hot. It's sometimes called hard-soldering because the solder, the
    brazing rod, is hard like brass, not soft like lead-tin solder. 
    Welding is entirely different; it's like melting two ice cubes then
    refreezing them as one cube.  They become one.  Of course this can
    all be described differently on a molecular level.  I am a
    professional welder certified in several diffent procedures.  

Ron

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project