    Hi Sandra, The conversion from wax to sterling is 1 to 10. I double
    checked specific gravities in Oppi Untracht's book: wax has a SG of
    .95-.98 and sterling is 10.4. I know this wasn't in your question, but
    I thought it might be helpful to those who carve a lot of waxes. I
    use my carat scale to weigh the waxes I'm carving and with a little
    high school math figured out the conversion: carat weight x .1286
    equals dwts. That obviously gives you the weight of the wax. Then I
    went a step further and multiplied .1286 by the specific gravity of
    the metal to be used. For example, the SG of 14K yellow is 13.07, so
    I multiply 13.07 by .1286 which equals 1.68. Personally I round it up
    to 1.8. Sooooooooooo, when I plunk my wax on the carat scale, I
    simply take the carat weight figure on the scale (say, 2.5 for an
    average ring for example) and multiply it by 1.8 and that immediately
    gives me a good idea of what it would weigh in gold (not including
    sprue). To simplify: -for 14K yellow: multiply weight of wax in carats
    by 1.8 -for 18K yellow: multiply by 2.0 -for platinum in general:
    multiply by 2.8 or so -for Sterling Silver: multiply by 1.3 Maybe
    others have found conversion numbers they prefer, but this works for
    me! 

Cindy 

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project