    Pam, This time I'm not exactly working on a ring, no.  I was asked to
    try to make a torus knot for a young lady out in Houston, a math
    major apparently, and before I got around to actually looking up what
    a torus knot _was_, I had come up with a toroidal knot that would be
    even better. 

    http://www.golden-knots.com/toroid.html 

    She likes the design, which is actually two torus knots tied in
    opposing directions in an over-one-under-one pattern, and I'm only
    going to charge her for the silver one I'll make after I figure out
    how . . .  so she won't be paying me for fifty hours of development
    and sore fingers and no sleep. I'll come out ahead anyway, since I'm
    going to make some in gold and market them to someone besides
    poverty-stricken students. 

    My dilemma is that I have to tie it on a core, and I have to remove
    the core without disturbing the wires. 

    This is going to be fun . . . 

Loren
http://www.golden-knots.com/

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project