>           Soldering copper IJS carries a wire solder, called Fos-Flo
>     #7, for copper. Item number is #801-WS, melt 1310f, flow 1350f.
>     Composition is 92.75% cu,  7.25% phosphorus. About 2 bucks for 20
>     feet. 

>         I've tried this solder with limited success.  it tends to
>     sizzle and sparkle rather than run into my seams.  i use my regular
>     sterling solder technique and flux...  anyone have any insights??
>     thanks  Mark Kaplan   markaplan AT hotmail.com 

    I have not tried it, but it has occurred to me -- has anyone tried
    using just the regular solder that  radio hams and suchlike use(d) to
    solder their wires? (before the days of printed circuits, etc.) It
    does, of course, have a silvery color, but  so does Fos-Flo #7. I
    think it's mostly lead, with a low melting point. 

Margaret

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project