========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== The biggest problem with Hydrogen/nitrogen as a heat source is the cost factor ...and the fact that you can easily fry small quantities of metal as the heat is extremely intense. You will go through roughly 4 to 5 times the amount of Hydrogen as you would propane which is the next cleanest gas... We use oxypropane and have excellent results ... the key factor here if you are getting good results with hydrogen and your results where not good using propane is based on the simple fact that the torch tip size you might have been using in the past was too small and you were not generating enough heat to bring your metal to a bright , clean state before casting. The best tip to use on your oxy propane torch is called a rose but tip... the bigger the better...The bigger it is, the faster your melt will be and you will have more than sufficient power to fry the metal to a crisp if this your intent..( which I do not suggest) also, the large rosebud tips have great , wide heat disipation and what this does is cover the entire top of the crucible , eliminating any oxygen from getting to the metal before casting. I have used hydrogen in the past so I am familiar with it and it does work, however, if you look at the tip on the end of you hydrogen torch, it is most likely a " Rosebud " tip... that should give you a clue ... We go through a singel 40 lbs tank of propane in about 1 month at a cost of approximately $23... In hydrogen gas, we would be using at Least $250 worth per month... So my advice is to think carefully about your old abandoned propane torch in the closet, take it out and put a BIG rose bud tip on it and save yourself a lot of money.... Daniel Grandi We do casting, finishing and a whole lot more for designers, jewelers, stores and people in the trade Contact of list at sales AT racecarjewelry.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project