    How about taking a silver or gold tube, drawing it thru a square
    drawplate  and sawing  it in half or drawing it thru a rectangle
    drawplate and cut or file off  the top. 

    Another idea would be to cut it in half with the Jump Ringer.      
    Calculate the height of two pieces of C-shaped channel plus the
    blade thickness, and use that to select the drawplate hole.  Draw it
    through a rectangle draw plate.  Use a pair of dividers to scribe 
    the center point on a side where you want to cut it.   Place it in a
    Jump Ringer , on top of a piece of wood, so you can cut all the way
    through.    Center it  using the scribe mark,  and cut it with the
    jump ringer ....(Ray, you can use this idea for a small
    percentage......<grin>......). 

Love and God Bless
-randy
Home 214-321-6253
Cell 214-280-7775
Work 469-775-6650
http://www.rocksmyth.com


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project