>       Removing  enamel Hi Phil, drop your piece of enamel in liquid
>     armor etch and wait.  It will eat away your glass and leave your
>     gold. Depending on the thickness of the enamel, it may take a day
>     or two. Lisa 
>
>         HI! Please let me know what is liquid armor?  I have tried
>     Blue Etch but it is too thick and is also very slow.  Thanks, Pat
>     DIACCA Topp 
>

    Sorry folks, missed out the ":" in the link in the previous post. 

    http://users.netconnect.com.au/~scratch/eNAMEL_hydrofluoric_acid.html

    is to an article that will run in the March issue of eNAMEL Online
    Newsletter. 

    Rather than wait I will make it available now.  There are issues of
    safety to be addressed with these materials. 

Al Heywood

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project